Polymer Property : Electrical Resistivity = 0.00000421 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000421 ohm-cm
0.00000421 ohm-cm
(41% IACS)
CMW® ELKONITE® 30W3 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12
For projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members. Information provided by CMW Inc.