Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® D1058 Silver Graphite Contact Material For electrical contacts, resistant to sliding wear.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material High wear resistance and reliability.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® ELKONITE® 50W3 Tungsten Copper material ASTM B702 For vacuum switch contacts.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® ELKONITE® 7165 Molybdenum Silver contact material For arcing electrical contactsInformation provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® THERMKON® 62 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Electrical Resistivity | <= 0.00000493 ohm-cm | <= 0.00000493 ohm-cm | Calculated from Min 35 %IACS |
Cadi Cu-Tungsten (80%) Copper Alloy Slightly higher tungsten content results in higher hardness and strength when forces are relatively high. Strength is gained with a slight decrease in electrical and thermal properties.Information .. |