Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000400 - 0.00000520 ohm-cm | 0.00000400 - 0.00000520 ohm-cm | |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Electrical Resistivity | 0.00000400 - 0.00000520 ohm-cm | 0.00000400 - 0.00000520 ohm-cm | |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |