Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 400 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 600 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Alpase K100-S™ Aluminum Plate K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corros.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 500 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Electrical Resistivity | 0.00000590 ohm-cm | 0.00000590 ohm-cm | |
Aleris Weldural Aluminum Alloy, 700 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |