Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.0000101 ohm-cm | 0.00000610 - 0.0000101 ohm-cm | 17-28% IACS Conductivity |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Electrical Resistivity | 0.00000610 - 0.0000101 ohm-cm | 0.00000610 - 0.0000101 ohm-cm | 17-28% IACS Conductivity |
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Electrical Resistivity | 0.00000610 - 0.0000101 ohm-cm | 0.00000610 - 0.0000101 ohm-cm | 17-28% IACS Conductivity |
Materion Beryllium Copper Alloy 190 Strip; SHM (TM05) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; over 76 mm o.d. (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000610 - 0.00000780 ohm-cm | 0.00000610 - 0.00000780 ohm-cm | 22-28% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |