Electrical Properties Metric English Comments
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000860 ohm-cm
0.00000688 - 0.00000860 ohm-cm
Conductivity is 20-25% IACS
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Electrical Resistivity 0.00000688 - 0.00000956 ohm-cm
0.00000688 - 0.00000956 ohm-cm
Conductivity is 18-25% IACS
Materion BrushCAST® 20CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..