Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000689 ohm-cm
0.00000689 ohm-cm
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite
Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate..