Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000840 ohm-cm | 0.00000840 ohm-cm | |
Lucas-Milhaupt BRAZE 401 Characteristics:Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc .. |
|||
Electrical Resistivity | 0.00000840 ohm-cm | 0.00000840 ohm-cm | |
Lucas-Milhaupt BRAZE 600 Silver Based Cadmium Free Filler Metal Characteristics: Braze 600 is a copper rich eutectiferous alloy, the eutectiferous portion of which is molten at 1300EF (705EC), about 25EF before the entire composition is completely fluid. Thus t.. |