Polymer Property : Electrical Resistivity = 0.00000948 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000948 ohm-cm
0.00000948 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Alloy 417 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire.
Electrical Resistivity 0.00000948 ohm-cm
0.00000948 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel A 200 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.