Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Hogen HM3000 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l..
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Indium Corp. Indalloy 128 Pure Tin
Information Provided by Indium Corporation
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy
Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not r..
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Mi-Tech Metals HD18 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm..
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy
Recommended for soldering to aluminum. Use flux #3. Zn causes high drossing, short shelf life as solder paste.Information provided by the manufacturer, Indium Corporation.
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Williams Advanced Alloys WS232 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Electrical Resistivity 0.0000110 - 0.0000160 ohm-cm
0.0000110 - 0.0000160 ohm-cm
Temperature Coefficient of 0.0006 to 0.0007/K
Goodfellow Phosphor Bronze
Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow.