Electrical Properties Metric English Comments
Electrical Resistivity 0.0000156 ohm-cm
0.0000156 ohm-cm
11 % IACS
CMW® ELKONIUM 43 palladium based alloy
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..
Electrical Resistivity 0.0000156 ohm-cm
0.0000156 ohm-cm
11 % IACS
CMW® ELKONIUM 72 gold based alloy
Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to ..