Electrical Properties Metric English Comments
Electrical Resistivity 0.0000220 ohm-cm
0.0000220 ohm-cm
Indium Corp. Indalloy 170 Pure Lead
Information Provided by Indium Corporation
Electrical Resistivity 0.0000220 ohm-cm
0.0000220 ohm-cm
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy
Very good resistance to alkaline corrosionInformation Provided by Indium Corporation