Polymer Property : Electrical Resistivity = 0.0000246 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm
(7% IACS Conductivity)
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica..
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm
(7% IACS Conductivity)
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm
(7% IACS Conductivity)
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.