Electrical Properties Metric English Comments
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, 1/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, Annealed
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, Extra Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, Extra Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Electrical Resistivity 0.0000324 ohm-cm
0.0000324 ohm-cm
Annealed
Eagle Brass 770 Nickel Silver 18%, Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..