Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.0000430 ohm-cm | <= 0.0000430 ohm-cm | 4% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way).. |
|||
Electrical Resistivity | <= 0.0000430 ohm-cm | <= 0.0000430 ohm-cm | 4% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Electrical Resistivity | <= 0.0000430 ohm-cm | <= 0.0000430 ohm-cm | 4% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Electrical Resistivity | <= 0.0000430 ohm-cm | <= 0.0000430 ohm-cm | 4% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way).. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy General purpose fusible alloy. Poor solderability.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Electrical Resistivity | 0.0000430 - 0.0000480 ohm-cm | 0.0000430 - 0.0000480 ohm-cm | Temperature Coefficient of 0.00001/K |
Goodfellow Manganin® Copper Resistance Alloy Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 302 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 306 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 33 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 34 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 41 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | 4 % IACS |
CMW® ELKONIUM 42 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
AK Steel DI-MAX® M-27 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | Fully Processed and Semi-Processed |
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | |
AIM 70 Fusible Alloy Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seal.. |
|||
Electrical Resistivity | 0.0000430 ohm-cm | 0.0000430 ohm-cm | (4% IACS Conductivity) |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |