Polymer Property : Electrical Resistivity = 0.0000450 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000450 ohm-cm
0.0000450 ohm-cm
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)
Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties..
Electrical Resistivity 0.0000450 ohm-cm
0.0000450 ohm-cm
Temperature Coefficient of 0.0034/K
Goodfellow Nickel 52/Iron 48 Alloy
Used in magnetic and glass-metal seal applicationInformation provided by Goodfellow.