Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000350 - 0.0000450 ohm-cm | 0.0000350 - 0.0000450 ohm-cm | Parallel (002) |
Mateck Highly Oriented Pyrolytic Graphite Oxidic single crystals. Applications include:Scanning tunneling microscopy-callibration and substratesGraphite monochromatorsx-ray diffractionneutron scattering and diffraction |
|||
Electrical Resistivity | 0.0000350 - 0.0000450 ohm-cm | 0.0000350 - 0.0000450 ohm-cm | parallel (002) direction |
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |