Polymer Property : Electrical Resistivity = 0.0000650 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000650 ohm-cm
0.0000650 ohm-cm
RT
Outokumpu 4028 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Electrical Resistivity 0.0000650 ohm-cm
0.0000650 ohm-cm
Kinetics MIM 12 Chrome
Stainless Steel for soft magnetic applications. Information provided by Kinetics, Inc.
Electrical Resistivity 0.0000650 ohm-cm
0.0000650 ohm-cm
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA
Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu..
Electrical Resistivity 0.0000650 ohm-cm
0.0000650 ohm-cm
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed
Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi..
Electrical Resistivity 0.0000650 ohm-cm
0.0000650 ohm-cm
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel
Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:..
Electrical Resistivity 0.0000650 ohm-cm

@Temperature 50.0 °C
0.0000650 ohm-cm

@Temperature 122 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..