Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000720 ohm-cm @Temperature 23.0 °C |
0.0000720 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 50% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 60% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 0% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, Annealed (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 30% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |