Electrical Properties Metric English Comments
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 100 °C
0.0000850 ohm-cm

@Temperature 212 °F
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Electrical Resistivity 0.0000850 ohm-cm
0.0000850 ohm-cm
RT
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Electrical Resistivity 0.0000850 ohm-cm
0.0000850 ohm-cm
RT
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Electrical Resistivity 0.0000850 ohm-cm
0.0000850 ohm-cm
RT
Outokumpu 4438 High Performance Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Electrical Resistivity 0.0000850 ohm-cm
0.0000850 ohm-cm
RT
Outokumpu 4439 Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms.
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 100 °C
0.0000850 ohm-cm

@Temperature 212 °F
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 100 °C
0.0000850 ohm-cm

@Temperature 212 °F
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 20.0 °C
0.0000850 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 20.0 °C
0.0000850 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Electrical Resistivity 0.0000850 ohm-cm

@Temperature 100 °C
0.0000850 ohm-cm

@Temperature 212 °F
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Copyright © lookpolymers.com All Rights Reserved