Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001039 ohm-cm @Temperature 23.0 °C |
0.0001039 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 20 Cb Plus Stainless Steel Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack.. |