Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000111 ohm-cm | 0.000111 ohm-cm | Temperature Factor is 1.10 at 800°C (1470°F). Temperature Factor is 1.11 at 1000°C (1830°F). Temperature Factor is 1.13 at 1200°C (2190°F). |
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |