Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001215 ohm-cm | 0.0001215 ohm-cm | |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |