Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000160 ohm-cm | 0.000160 ohm-cm | |
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i.. |