Electrical Properties Metric English Comments
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm
(x-y); ASTM-C611 (4-Point Resistivity Test)
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm
(x-y); ASTM-C611 (4-Point Resistivity Test)
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm
(x-y); ASTM-C611 (4-Point Resistivity Test)
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm
UCAR Carbon UCAR® SLX Extruded Graphite
Densified prior to graphitization, Grade SLX is an extruded graphite with increased densities and strength over SL.Typical Applications:CZ silicon crystal growth Quartz processing Purified electroni..
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm
Cytec Thornel® P-75S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the i..