Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000840 ohm-cm | 0.000840 ohm-cm | |
UCAR Carbon UCAR® CBY Extruded Graphite Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.Typical App.. |