Polymer Property : Electrical Resistivity = 0.000850 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000850 ohm-cm
0.000850 ohm-cm
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla..