Electrical Properties Metric English Comments
Electrical Resistivity 0.00142 ohm-cm
0.00142 ohm-cm
Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Electrical Resistivity 0.00142 ohm-cm
0.00142 ohm-cm
Cytec Thornel® T-650/42 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..