Electrical Properties Metric English Comments
Electrical Resistivity 1.29e+16 ohm-cm
1.29e+16 ohm-cm
Abatron AboCast 50-6/AboCure 50-12 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Colorless. Shelf life is 12+ months.