Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.60e+13 ohm-cm | 1.60e+13 ohm-cm | |
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |