Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.75 ohm-cm | 1.75 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.75 ohm-cm | 1.75 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.75 ohm-cm | 1.75 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.75 ohm-cm | 1.75 ohm-cm | particle 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.75 ohm-cm | 1.75 ohm-cm | Particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |