Polymer Property : Electrical Resistivity = 1.90e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.90e+11 - 1.74e+15 ohm-cm
1.90e+11 - 1.74e+15 ohm-cm
Average value: 1.77e+14 ohm-cm Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..