Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00 - 2.00e+13 ohm-cm | 1.00 - 2.00e+13 ohm-cm | Average value: 1.25e+12 ohm-cm Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+13 - 2.00e+13 ohm-cm | 1.00e+13 - 2.00e+13 ohm-cm | Average value: 1.20e+13 ohm-cm Grade Count:5 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |