Polymer Property : Electrical Resistivity = 2.30e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.30e+14 ohm-cm
2.30e+14 ohm-cm
ASTM D257
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Electrical Resistivity 2.30e+14 ohm-cm
2.30e+14 ohm-cm
ASTM D257
CRP Technology Windform® FX Polyamide Composite
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive..