Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+9 - 2.30e+17 ohm-cm | 1.00e+9 - 2.30e+17 ohm-cm | Average value: 4.72e+16 ohm-cm Grade Count:59 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |