Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3.10e+15 ohm-cm | 3.10e+15 ohm-cm | |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |