Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3000 - 1.00e+17 ohm-cm | 3000 - 1.00e+17 ohm-cm | Average value: 1.56e+16 ohm-cm Grade Count:56 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Electrical Resistivity | 3000 - 4.00e+15 ohm-cm | 3000 - 4.00e+15 ohm-cm | Average value: 1.64e+15 ohm-cm Grade Count:7 |
Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 3000 ohm-cm | 3000 ohm-cm | |
Ceradyne CeraTrex™ SC-P3 Silicon Carbide Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company |
|||
Electrical Resistivity | 3000 ohm-cm | 3000 ohm-cm | |
BASF Sicotan® Brown K 2611 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |