Electrical Resistivity 3600 ohm-cm
3600 ohm-cm
BASF Sicotan® Yellow K 2001 F Color Additive
Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B..