Electrical Properties Metric English Comments
Electrical Resistivity 4.70e+12 - 1.20e+13 ohm-cm
4.70e+12 - 1.20e+13 ohm-cm
Average value: 8.35e+12 ohm-cm Grade Count:6
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Electrical Resistivity 4.70e+12 ohm-cm
4.70e+12 ohm-cm
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Electrical Resistivity 4.70e+12 ohm-cm
4.70e+12 ohm-cm
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Electrical Resistivity 4.70e+12 ohm-cm
4.70e+12 ohm-cm
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..