Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Electrical Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Electrical Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
3M Fluorinert™ FC-3283 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor.. |
|||
Electrical Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
Electrical Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |