Electrical Properties Metric English Comments
Electrical Resistivity 2.50 - 5.60e+15 ohm-cm
2.50 - 5.60e+15 ohm-cm
Average value: 3.94e+14 ohm-cm Grade Count:43
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Electrical Resistivity 2.50 - 5.60e+15 ohm-cm
2.50 - 5.60e+15 ohm-cm
Average value: 5.77e+14 ohm-cm Grade Count:204
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..