Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+12 ohm-cm | 6.00e+12 ohm-cm | Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity) |
Cytec Conathane® CC-1155 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 6.00e+12 ohm-cm | 6.00e+12 ohm-cm | Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity) |
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 6.00e+12 ohm-cm | 6.00e+12 ohm-cm | Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity) |
Cytec Conathane® CC-1195 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |