Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+13 ohm-cm | 6.00e+13 ohm-cm | ASTM D257 |
Toyobo Pelprene™ P-70B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |