Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.97e+16 ohm-cm | 6.97e+16 ohm-cm | ASTM D257 |
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |