Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 700 ohm-cm | 700 ohm-cm | 4.1% graphite |
TIMCAL TIMREX® MB25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |