Dielectric Breakdown >= 13000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 13000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 41 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe.
Dielectric Breakdown >= 13000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 13000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 41 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe.