Electrical Properties Metric English Comments
Dielectric Breakdown >= 30000 V

@Temperature 90.0 - 90.0 °C
>= 30000 V

@Temperature 194 - 194 °F
Average value: 30000 V Grade Count:1
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
Dielectric Breakdown >= 30000 V

@Time 20.0 - 60.0 sec
>= 30000 V

@Time 0.00556 - 0.0167 hour
Average value: 30000 V Grade Count:1
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
Dielectric Breakdown 30000 V

@Thickness 1.57 mm
30000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 24 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in electrical and mechanical applications. Very good electrical properties when exposed to high relative humidity. Much higher mechanical strength and insulation resistance than type PF CP 21..
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 24 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in electrical and mechanical applications. Very good electrical properties when exposed to high relative humidity. Much higher mechanical strength and insulation resistance than type PF CP 21..
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF ..
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF ..
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe SI GC 41 Woven Glass Cloth Reinforced Silicone Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe.
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe SI GC 41 Woven Glass Cloth Reinforced Silicone Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe.
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe.
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe.
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe.
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe.