Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Condition A |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Dielectric Breakdown | 65000 V @Thickness 1.57 mm |
65000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP318 Cotton Fabric Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t.. |