Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 66000 V @Thickness 1.57 mm |
66000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |