Electrical Properties Metric English Comments
Surface Resistivity per Square 0.014 ohm

@Temperature 85.0 °C,
Time 605000 sec
0.014 ohm

@Temperature 185 °F,
Time 168 hour
Final; CHO-TM-TP57
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Surface Resistivity per Square 0.014 ohm

@Temperature 85.0 °C,
Time 605000 sec
0.014 ohm

@Temperature 185 °F,
Time 168 hour
Final; CHO-TM-TP57
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Surface Resistivity per Square 0.014 ohm

@Temperature 85.0 °C,
Time 605000 sec
0.014 ohm

@Temperature 185 °F,
Time 168 hour
Final; CHO-TM-TP57
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Surface Resistivity per Square 0.014 ohm

@Temperature 85.0 °C,
Time 605000 sec
0.014 ohm

@Temperature 185 °F,
Time 168 hour
Final; CHO-TM-TP57
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Surface Resistivity per Square 0.014 ohm

@Temperature 85.0 °C,
Time 605000 sec
0.014 ohm

@Temperature 185 °F,
Time 168 hour
Final; CHO-TM-TP57
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Copyright © lookpolymers.com All Rights Reserved